ZHONGSHAN BORIS PRINTING INK CO., LTD

Favorite  |  Set Home
skype: boris198402
QQ: 523414211
FACEBOOK: https://www.facebook.com/boris.yang.33
E-mail: https://www.linkedin.com/in/boris-yang-2ba217104/
E-mail: info@borisprintingink.com
Contact Us

Name: Boris Yang
Tel: +86 760 86369515
Mobile: +86 15819802587
E-mail: info@borisprintingink.com
E-mail: Borisprintingink@aliyun.com
Add: Vigour Creative Park, Sanxiang Town, Zhongshan, China
Skype: boris198402
WeChat: +86 15819802587
whatsapp: +86 15819802587
QQ: 523414211
Skype: boris198402 facebook: https://www.facebook.com/boris.yang.33 QQ: 523414211 info@borisprintingink.com Borisprintingink@aliyun.com

Product name : Nylon screen ink
Product No. : SNCC series
←[Previous Product]              [Next Product]→
Online Inquiry         Email Us

  Details:

                                         Gloss Nylon ink


1.
Substrates:

Waterproof nylon fabricnon-waterproof fabricluggage fabric Oxford fabric and nylon plastic.

 

2. Product features:
High glossgood softnessstrong coveragegood adhesion on high waterproof nylon fabric.

                                                       

3. Test items&results:

Adhesion: good

Scratch resistance: 4-5

Wear resistance: 4-5

Crumpling resistance: 5

Acid resistance: 4-5

Alkali resistance: 4-5

Wash resistance: 3-4

Migration resistance: 4-5

 

4. Technical parameters:

Color shade: refer to color card

 Color concentration:8-15%

 

Fineness:7um

Viscosity: 200-280p

Gloss: 75-85

Liquidity: 10-15mm/s

Solid content: 45%

 

 

5. Instructions:

(1) Mesh: 150-350 polyester mesh

(2) Squeegee: Polyurethane squeegee at the hardness 65-85 is recommended.

(3) Indicative dosage: 30/ on the 200 mesh

(4) Drying: natural drying (surface drying in 7-15 mins, full drying in more than 24 hours) or blow drying at temperature below 100.

(5) Selective Solvents: quick drying water 719, medium drying water 718 or  cyclohexanone based on printing conditions.

 

(6) Stencil cleaning: organic solvent (e.g. stencil cleaning water)

6. Notes:

(1) Please pay attention to the solvents dissolving capacity while diluting the ink.

 

(2) It will cause pattern scratch by the stack of finished press works on PVC film due to the PVCs poor solvent resistance. So pay attention to the drying status of ink when finish work and avoid excessive overlap.

 

(3) Color migration will occur while printing on PVC film containing a lot of plasticizers. The printing ink with good anti-permeability is recommended.

 

(4) The rigorous sample test before use is necessary to check the printing inks adhesion on different waterproof nylon fabrics.

 

(5) The catalyst 9004 should be added appropriately (by 5-8%) into the ink to improve adhesion when printing on waterproof nylon fabric. But the printing ink with added catalyst must be finished within 8 hours, or will be scrapped.

7. Storage:

It can be stored for 36 months at 5-35℃. Keep away from strong light. Avoid strong acid and strong alkali.

8. Remarks:

(1) Please thoroughly read the instructions and make a sample test before use.

(2) The technical data is for reference only.

THE END


  Related Products :

SNC(C)-306 ORANGE RED
SNC(C)-306 ORANGE RED

5KG/CAN, 20KG/CARTON
5KG/CAN, 20KG/CARTON

PP INK
PP INK

ZY-175 RICH GOLD POWDER(7UM)
ZY-175 RICH GOLD POWDER(7UM)

Balloon ink
Balloon ink

Gloss PVC ink(Rich Gold)
Gloss PVC ink(Rich Gold)

PVC INK
PVC INK

PVC INK(LESS SMELL)
PVC INK(LESS SMELL)

Online service

Skype: boris198402 523414211 info@borisprintingink.com Borisprintingink@aliyun.com

Wechat

+86 15819802587